Fibre: |
100% Polyester |
Scrim: |
100% Polyester |
Basis Weight: |
500-600 g/m2 |
Permeability: |
25 - 35 ft3/ft2.min (cfm) at ½" w.g. pressure |
|
7.6 – 10.7 m3/m2.min at 127Pa pressure |
Media Finishes Available: |
Singed, Smooth, PTFE impregnated, or with ePTFE membrane |
Maximum Recommended Continuous Dry Operating Temperature: |
132℃ |
Maximum Short Term Surge Temperature: |
150℃ |
Maximum Recommended Continuous Moist Operating Temperature: |
94℃ |
Chemical Resistance: |
Acids |
- Fair |
|
Alkalis |
- Fair |
|
Oxidising Agents |
- Good |
Note: polyester media may be attacked by moist heat hydrolysis, strong acids, or strong alkalis. To avoid such occurrences please operate in an environment in accordance with the above recommendations.
|